Multi Jet Fusion (MJF), selective laser sintering (SLS), and fused deposition modeling (FDM) are the three most common plastic 3D printing processes. MJF and SLS both fuse nylon powder in a heated bed and produce strong, functional parts without support structures. FDM extrudes melted filament and trades strength and surface finish for a lower cost of entry. The right choice comes down to part geometry, quantity, mechanical requirements, and how the part will actually be used.

Here’s how the three processes work, where each one wins, and where each one falls short.
Multi Jet Fusion is HP’s powder bed fusion technology. An inkjet array deposits a fusing agent onto a thin layer of nylon powder wherever the part’s cross-section sits, plus a detailing agent along the edges to keep features crisp. Infrared lamps then pass over the full bed, and the powder under the fusing agent absorbs that energy and melts into a solid layer. The bed drops by roughly 80 microns, fresh powder sweeps across, and the cycle repeats. HP’s technical documentation covers how these functional agents control fusing at the voxel level.

Two things make this process fast and consistent. First, the infrared lamps fuse an entire layer in a single pass, so a full build of nested parts takes about as long as a single part. Second, the surrounding unfused powder supports every overhang and internal channel, which means no support structures to design around or break off.
MJF parts print in gray because the fusing agent contains carbon. Dyeing produces a deep, uniform black. Mechanical properties are near-isotropic, meaning the part performs about the same regardless of print orientation.
Selective laser sintering fuses nylon powder with a CO2 laser instead of agents and lamps. The laser traces each layer’s cross-section point by point, sintering the powder just below its melting temperature. Typical SLS layers run 100 to 120 microns. Like MJF, the unfused powder acts as support, so complex geometry prints without added structures.
SLS is the older of the two powder processes and has a broad installed base. Its material catalog is wider in some categories, including PA11 and glass-filled nylons on many machines, and some SLS platforms offer larger build volumes than MJF’s roughly 380 x 284 x 380 mm chamber. SLS PA12 parts print white or off-white, which takes color dyes more readily than gray MJF stock.
Fused deposition modeling melts a thermoplastic filament and extrudes it through a nozzle, drawing each layer like a very precise hot glue gun. It’s the most accessible 3D printing process and the cheapest way to get a single prototype in hand.
The tradeoff is structural. FDM parts are anisotropic: layers bond where melted plastic meets cooled plastic, and that bond is the weak point. Load a part along its Z axis and it can delaminate. Visible layer lines also mean FDM surfaces need sanding or coating for anything customer-facing. Where FDM earns its keep is quick fit checks, jigs and fixtures under light load, very large parts on big-format machines, and high-temperature materials like ULTEM (PEI) that standard nylon powder bed systems don’t run.
MJF and SLS produce parts that look similar on a spec sheet. The differences show up in speed, surface, economics, and color.
| MJF | SLS | FDM | |
|---|---|---|---|
| Fusion method | Fusing agent + infrared lamps | CO2 laser | Extruded filament |
| Typical layer height | ~80 microns | 100 to 120 microns | 100 to 300 microns |
| Support structures | None needed | None needed | Required for overhangs |
| Mechanical behavior | Near-isotropic | Near-isotropic | Anisotropic, weak in Z |
| As-printed surface | Slightly grainy, gray | Slightly grainy, white | Visible layer lines |
| Best fit | Functional parts, production runs | Specialty nylons, large builds | Prototypes, jigs, large simple parts |
Speed at volume. MJF fuses whole layers at once; SLS traces them with a laser. Pack a build chamber full of parts and MJF finishes sooner, which shortens lead times on production quantities.
Detail and edges. MJF’s detailing agent sharpens the boundary between fused and unfused powder, holding cosmetic features down to 0.5 mm. Structural walls want 0.8 to 1.0 mm, covered in the tolerance section below.
Powder economics. HP specifies up to 80 percent reusability for surplus MJF PA12 powder. Typical SLS refresh rates for PA12 run meaningfully lower. Less virgin powder per build feeds directly into per-part cost on repeat production.
Color. SLS prints white and dyes to a range of colors. MJF prints gray and dyes best to black. If a specific non-black color is a hard requirement, that pushes the decision.
T5 Innovation holds ±0.3 mm on features up to 100 mm, and ±0.3 percent of nominal above that. More useful than the number is knowing where accuracy degrades, because it isn’t where most engineers expect.
Tom Tillges, co-owner of T5 Innovation, puts it plainly: “Large flats are number one, not thin walls, which is what people expect.” A long unsupported flat span contracts unevenly on cooldown and bows. Past about 150 mm of flat span, plan for it: orient the part off-axis in the build, add ribbing, or split the geometry.
Second is where the part sits in the build, not how tall it is. Z is actually the well-behaved axis in MJF. The real variable is thermal history. A part near the chamber wall sees different conditions than one in the center, which is why the same file can measure slightly differently between two builds.
Thin walls come third. T5 treats 0.8 to 1.0 mm as the structural minimum, with 0.5 mm reserved for cosmetic, non-load features. Below 0.7 mm, incomplete fusion becomes a risk.
One more thing worth knowing before you send a file: holes print undersize. A 5 mm hole typically measures 4.8 to 4.9 mm, so T5 either oversizes it in CAD or reams it as a secondary operation. As Tom says: “We tell people that before the build, not after.”
FDM wins on a single quick prototype. The machine time is cheap and there’s no powder bed to fill, cool, and unpack.
The math flips as quantity grows. Powder bed processes nest dozens or hundreds of parts in one build with no per-part tooling, and MJF’s full-layer fusing plus high powder reuse gives it the edge on cost per part from prototype quantities into the thousands of units. That’s the territory where teams historically waited on injection mold tooling. MJF fills it without the tooling spend, and design changes between batches cost nothing.
Cooling time is the hidden line item in powder bed quotes. A dense MJF or SLS build needs controlled cooling before parts come out, so a quoted lead time covers print, cool, depowder, and finish, not just print.
As-printed powder bed parts have a matte, slightly grainy surface. For many industrial applications that’s fine. When it isn’t, post-processing closes the gap.
Vapor smoothing exposes the part to a solvent vapor that reflows the outer skin into a smooth, sealed finish. The real payoff isn’t cosmetic. As-printed MJF is porous; a smoothed part has a closed surface that resists moisture and chemical ingress and can actually be cleaned, which is the argument that matters for medical, orthotic, and other hygiene-sensitive parts.
Two things to know before smoothing a part. Dimensional change is small: the process redistributes surface material rather than removing it, typically under 10 to 20 microns, which sits inside the process tolerance band. Edge rounding is real, though. Sharp corners pick up a small radius, and embossed or engraved text below about half a millimeter loses definition. If a design depends on a crisp edge or molded-in branding, flag it before the part gets smoothed.
MJF is not the answer to every part, and T5 says so when it isn’t. The cases where a part gets steered elsewhere:

T5 Innovation is an additive manufacturing service bureau in St. Paul, Minnesota, specializing in HP Multi Jet Fusion. We made that bet deliberately: for functional nylon parts from one-off prototypes through production runs, MJF delivers the most consistent combination of mechanical performance, per-part cost, and repeatability.
Everything runs fully in-house. We print PA12 and TPU, both dyeable, and finish parts on an AMT PostPro vapor smoothing system. There are no order minimums, so a single prototype and a thousand-unit production run get the same process and the same quality system, certified to ISO 9001 and ISO 13485. T5 is ITAR registered and a member of the HP Partner Additive Manufacturing Network.
Three lead time tiers cover most schedules: expedited at about 48 hours, standard at 3 to 5 days, and economy at 5 to 10 days.
Have a part in hand and not sure which process fits? Send us the model. We’ll tell you straight whether MJF is the right tool for it, and quote it if it is. Get a quote from T5 Innovation.